Centrifugal Casting Alloy Indefinite Chilled Roll

image_pdfimage_print

Centrifugal Casting Alloy Indefinite Chilled Roll

Indefinite chilled cast iron roll

The outer layer exhibits a remarkable mechanical performance and the quantity of graphite in the roll work layer remains basically unchanged along the depth, producing therefore no adverse effect on the decrease of hardness of work layer. The hardness of roll depends mainly on type of matrix (sorbite, bainite, martensite).

Centrifugal Casting Alloy Indefinite Chilled Roll

Mechanical properties

Hardness of shell                HSD60-85
Hardness of core                HSD35-48
Tensile Strength of core                ≥450MPa

Chemical properties

Material

Hardness (HSD)

C

Si

Mn

Ni

Cr

Mo

Indefinite I

60-70

3.0/3.5

0.5/1.0

0.5/1.0

0.5/1.0

0.5/1.0

0.2/0.6

Indefinite II

62-72

3.0/3.5

0.5/1.0

0.5/1.0

1.0/2.0

0.5/1.0

0.2/0.6

Indefinite III

65-75

3.0/3.5

0.5/1.0

0.5/1.0

2.0/3.0

0.7/1.2

0.2/0.6

Indefinite IV

70-80

3.0/3.5

0.5/1.0

0.5/1.0

3.0/5.0

1.0/2.0

0.2/0.6

Application